Fabrication of ZrO-Bearing lithium-silicate glass-ceramics by pressureless sintering and spark plasma sintering.

Title Fabrication of ZrO-Bearing lithium-silicate glass-ceramics by pressureless sintering and spark plasma sintering.
Authors M. Ghayebloo; P. Alizadeh; R.M. Melo
Journal J Mech Behav Biomed Mater
DOI 10.1016/j.jmbbm.2020.103709
Abstract

OBJECTIVE: the present study evaluated the effect of the Spark Plasma Sintering (SPS) and Pressureless Sintering (PLS) methods on the physical and mechanical properties of ZrO-bearing Lithium Silicate (ZLS) glass-ceramics.

METHOD: SPS and PLS methods were used for fabricating of the zirconia-bearing Lithium Silicate glass-ceramics. Several sintering temperatures were applied in order to achieving the best mechanical and physical properties in both methods. For this purpose, the particle size measurement of the glass powder was performed. Field Emission Scanning Electron Microscope (FESEM) was carried out for evaluation of the microstructure. X-ray diffraction (XRD) was used to investigate the amorphous or crystalline state of the samples. Fourier Transform Infrared Spectroscopy (FTIR) was used for the investigation of the chemical bonds. Flexural strength, Vickers microhardness, fracture toughness, and physical properties such as bulk density, water absorption, and the apparent porosity of the samples were measured.

RESULTS: It is possible to fabricate ZLS glass-ceramics by the SPS method at a sintering temperature approximately 350 °C lower than the sintering temperature of the PLS method. Results of the SPS showed SGC, 550 °C (SPS Glass Ceramic sintered at 550 °C) had the highest flexural strength (255.10 ± 15.44 MPa), fracture toughness (3.15 ± 0.62 MPam), Vickers microhardness (7.96 ± 0.13 GPa) and bulk density (2.63 ± 0.02 g/cm); the lowest water absorption (0.11 ± 0.12) and, apparent porosity (0.25 ± 0.32). Results of the PLS showed PLGC, 900 °C (PLS Glass Ceramic sintered at 900 °C) had the flexural strength (160.27 ± 12.69 MPa), the highest Vickers microhardness (7.22 ± 0.67 GPa) and bulk density (2.53 ± 0.03 g/cm); the lowest water absorption (0.15 ± 0.21) and, apparent porosity (0.39 ± 0.54). According to the XRD patterns and FESEM images, SGC, 550 °C has LiSiO spherical nanocrystals (approximately 50-100 nm diameters).

SIGNIFICANCE: Different sintering temperatures in the SPS and PLS methods have an obvious effect on the microstructure, mechanical, and physical properties of ZrO-bearing Lithium Silicate (ZLS) glass-ceramics. Sintering temperature was decreased in SPS compared to the PLS method and nanocrystals of LiSiO formed.

Citation M. Ghayebloo; P. Alizadeh; R.M. Melo.Fabrication of ZrO-Bearing lithium-silicate glass-ceramics by pressureless sintering and spark plasma sintering.. J Mech Behav Biomed Mater. 2020;105:103709. doi:10.1016/j.jmbbm.2020.103709

Related Elements

Lithium

Lithium Bohr ModelSee more Lithium products. Lithium (atomic symbol: Li, atomic number: 3) is a Block S, Group 1, Period 2 element with an atomic weight of 6.94. The number of electrons in each of Lithium's shells is [2, 1] and its electron configuration is [He] 2s1. The lithium atom has a radius of 152 pm and a Van der Waals radius of 181 pm. Lithium was discovered by Johann Arvedson in 1817 and first isolated by William Thomas Brande in 1821. The origin of the name Lithium comes from the Greek wordlithose which means "stone." Lithium is a member of the alkali group of metals. It has the highest specific heat and electrochemical potential of any element on the period table and the lowest density of any elements that are solid at room temperature. Elemental LithiumCompared to other metals, it has one of the lowest boiling points. In its elemental form, lithium is soft enough to cut with a knife its silvery white appearance quickly darkens when exposed to air. Because of its high reactivity, elemental lithium does not occur in nature. Lithium is the key component of lithium-ion battery technology, which is becoming increasingly more prevalent in electronics.

Silicon

See more Silicon products. Silicon (atomic symbol: Si, atomic number: 14) is a Block P, Group 14, Period 3 element with an atomic weight of 28.085. Silicon Bohr MoleculeThe number of electrons in each of Silicon's shells is 2, 8, 4 and its electron configuration is [Ne] 3s2 3p2. The silicon atom has a radius of 111 pm and a Van der Waals radius of 210 pm. Silicon was discovered and first isolated by Jöns Jacob Berzelius in 1823. Silicon makes up 25.7% of the earth's crust, by weight, and is the second most abundant element, exceeded only by oxygen. The metalloid is rarely found in pure crystal form and is usually produced from the iron-silicon alloy ferrosilicon. Elemental SiliconSilica (or silicon dioxide), as sand, is a principal ingredient of glass, one of the most inexpensive of materials with excellent mechanical, optical, thermal, and electrical properties. Ultra high purity silicon can be doped with boron, gallium, phosphorus, or arsenic to produce silicon for use in transistors, solar cells, rectifiers, and other solid-state devices which are used extensively in the electronics industry.The name Silicon originates from the Latin word silex which means flint or hard stone.

Related Forms & Applications