Atomic Layer Deposition of Lithium Niobium Oxides as Potential Solid-State Electrolytes for Lithium-Ion Batteries.

Title Atomic Layer Deposition of Lithium Niobium Oxides as Potential Solid-State Electrolytes for Lithium-Ion Batteries.
Authors B. Wang; Y. Zhao; M.Norouzi Banis; Q. Sun; K.R. Adair; R. Li; T.K. Sham; X. Sun
Journal ACS Appl Mater Interfaces
DOI 10.1021/acsami.7b13467
Abstract

The development of solid-state electrolytes by atomic layer deposition (ALD) holds unparalleled advantages toward the fabrication of next-generation solid-state batteries. Lithium niobium oxide (LNO) thin films with well-controlled film thickness and composition were successfully deposited by ALD at a deposition temperature of 235 °C using lithium tert-butoxide and niobium ethoxide as Li and Nb sources, respectively. Furthermore, incorporation of higher Li content was achieved by increasing the Li-to-Nb subcycle ratio. In addition, detailed X-ray absorption near edge structure studies of the amorphous LNO thin films on the Nb L-edge revealed the existence of Nb as Nb5+ in a distorted octahedral structure. The octahedrons in niobium oxide thin films experienced severe distortions, which could be gradually alleviated upon the introduction of Li atoms into the thin films. The ionic conductivities of the as-prepared LNO thin films were also measured, with the highest value achieving 6.39 × 10-8 S cm-1 at 303 K with an activation energy of 0.62 eV.

Citation B. Wang; Y. Zhao; M.Norouzi Banis; Q. Sun; K.R. Adair; R. Li; T.K. Sham; X. Sun.Atomic Layer Deposition of Lithium Niobium Oxides as Potential Solid-State Electrolytes for Lithium-Ion Batteries.. ACS Appl Mater Interfaces. 2018. doi:10.1021/acsami.7b13467

Related Elements

Niobium

See more Niobium products. Niobium (atomic symbol: Nb, atomic number: 41) is a Block D, Group 5, Period 5 element with an atomic weight of 92.90638. Niobium Bohr ModelThe number of electrons in each of niobium's shells is 2, 8, 18, 12, 1 and its electron configuration is [Kr] 4d4 5s1. The niobium atom has a radius of 146 pm and a Van der Waals radius of 207 pm. Niobium was discovered by Charles Hatchett in 1801 and first isolated by Christian Wilhelm Blomstrand in 1864. In its elemental form, niobium has a gray metallic appearance. Niobium has the largest magnetic penetration depth of any element and is one of three elemental type-II superconductors (Elemental Niobiumalong with vanadium and technetium). Niobium is found in the minerals pyrochlore, its main commercial source, and columbite. The word Niobium originates from Niobe, daughter of mythical Greek king Tantalus.

Lithium

Lithium Bohr ModelSee more Lithium products. Lithium (atomic symbol: Li, atomic number: 3) is a Block S, Group 1, Period 2 element with an atomic weight of 6.94. The number of electrons in each of Lithium's shells is [2, 1] and its electron configuration is [He] 2s1. The lithium atom has a radius of 152 pm and a Van der Waals radius of 181 pm. Lithium was discovered by Johann Arvedson in 1817 and first isolated by William Thomas Brande in 1821. The origin of the name Lithium comes from the Greek wordlithose which means "stone." Lithium is a member of the alkali group of metals. It has the highest specific heat and electrochemical potential of any element on the period table and the lowest density of any elements that are solid at room temperature. Elemental LithiumCompared to other metals, it has one of the lowest boiling points. In its elemental form, lithium is soft enough to cut with a knife its silvery white appearance quickly darkens when exposed to air. Because of its high reactivity, elemental lithium does not occur in nature. Lithium is the key component of lithium-ion battery technology, which is becoming increasingly more prevalent in electronics.

Related Forms & Applications